Shoutout to the guys who say you can't fight a cold joint, because a 90 degree pour in Tucson proved me wrong
Everyone in my crew swears a cold joint means tear it out and start over, but last August on a driveway pour off Speedway we hit 104 degrees and the truck sat for 40 minutes. I kept the joint wet and worked the edge slow, and that seam is still tight 4 months later. Took me about 3 hours longer than a normal pour and I got plenty of grief for it. Am I crazy for thinking a cold joint done patient beats a rushed hot one, or does somebody have a story where it fell apart?