Hot take: old timer on the job in Beaumont told me to preheat 309L stainless slower than carbon, and I ignored him
Back in 2022 I was welding some 309L overlay on a tank and this old timer named Ray told me to bump my preheat way up and keep it slow between passes, said the cracks would show up later if I rushed it. I figured he was just stuck in his ways and ran it like I always do with carbon, 2 passes and move on. About 3 weeks after we hydro tested, we got hairline cracks in two spots right at the toe of the weld and had to grind it all out. Boss pulled the procedure sheet and turns out Ray was dead on about the preheat range and my interpass temps were way under spec. Cost us about 16 hours of rework on a Friday night. Any of you run into that where the old school guy is right and the shortcut costs you? Curious how you handle preheat on 309L overlay jobs.