My forge weld on a 5 layer billet split down the seam last Thursday, do you flux the whole stack or just the faces?
Half the guys I talk to say flux every layer or you get cold shuts, the other half say flux just makes a mess and a clean grind plus borax on the outside is all you need, so which side are you on?